Diffusion lengths of silicon solar cells from luminescence images (2007)

Würfel, P., Trupke, T., Puzzer, T., Schäffer, E., Warta, W., Glunz, S.W.

A method for spatially resolved measurement of the minority carrier diffusion length in silicon wafers and in silicon solar cells is introduced. The method, which is based on measuring the ratio of...

Investigation of structured TiAIN- and TiO2-coatings with moth-eye-like surface morphologies (2005)

Burmeister, F., Schäffer, E., Kleer, G., Döll, W., Bläsi, B., Gombert, A.

This paper is to report on the development and investigation of a specific type of growth mode and surface morphology of PVD-coatings, namely a columnar growth mode where the individual columns are...

Grundlegende Untersuchungen zur Erniedrigung der Klebeneigung zwischen Kunststoffen und Formmaterialien (2005)

Kleer, G., Könczöl, L., Schäffer, E., Schlögl, S.

Verminderte Werkzeugstandzeiten, lange Prozesszyklen und erhöhter Reinigungsaufwand erweisen sich als Haupthindernisse für die Anwendung neuer, leistungsfähiger Kunststoffprodukte sowie für das...

Grundlegende Untersuchungen zur Erniedrigung der Klebeneigung zwischen Kunststoffen und Formmaterialien (2004)

Kleer, G., Schäffer, E., Schlögl, S.

Verminderte Werkzeugstandzeiten, lange Prozesszyklen und erhöhter Reinigungsaufwand erweisen sich als Haupthindernisse für die Anwendung neuer, leistungsfähiger Kunststoffprodukte sowie für das...

Capillary instabilities by fluctuation induced forces (2003)

Morariu, M D, Schäffer, E., Steiner, U.

The spontaneous break-up of thin films is commonly attributed to the destabilizing effect of van-der Waals forces. Dispersion forces can be considered in terms of the confinement of the...

Composite coating materials for the moulding of diffractive and refractive optical components of inorganic glasses (2003)

Hock, M., Schäffer, E., Döll, W., Kleer, G.

The application of glass moulding processes to the fabrication of microoptical components is up to now limited by the problem of sticking between the aggressive glass melts and the moulding tools. In...

Composite coating materials for the hot embossing of microoptical components in inorganic glasses (2003)

Kleer, G., Döll, W., Hock, M., Manns, P., Schäffer, E.

In future technologies of telecommunication and laser techniques there is a high demand on microoptical components having aspherical or fresnel- and grid-shaped surfaces. For many of these components...

Temperature-gradient-induced instability in polymer films (2002)

Schäffer, E., Harkema, S., Blossey, R., Steiner, U.

We report the experimental observation and a theoretical model for a thin-film instability caused by a temperature gradient. A polymer-air double layer sandwiched between two plates set to different...